Polycarbonate (PC)

D451RC

Manufacturer:LNP™ THERMOCOMP™

高模量,低翘曲,良好的延展性,非溴化、非氯化阻燃剂,回收消费后(PCR)聚碳酸酯含量高达35%

Recorded properties

Record date:2026-11-07

PropertyValueUnit
Density1.52g/cm³
Melt flow rate69.0g/10min
Tensile strength140.0MPa
Tensile modulus11800.0MPa
Elongation at break1.9%
Flexural modulus10700.0MPa
Notched impact strength12.0kJ/m²
HDT 1.8MPa112.0°C
HDT 0.45MPa118.0°C
Vicat softening point123.0°C
Flame ratingV-0 class—

Test standard, specimen condition and source rights are not fully recorded. Values are for preliminary screening only; verify with the manufacturer before design or purchasing decisions.

Grade handling information to verify

The information below was automatically extracted from a material PDF and has not been individually reviewed. It is for preliminary reference only. Verify the exact grade’s manufacturer processing instructions, safety data sheet and equipment procedures before production; do not use candidate values directly as machine settings.

Matched by original PDF filename

Storage
Review the source for packaging, storage and opened-package instructions.
Drying
Candidate injection-molding recommendations: temperature 110 °C; time 3 - 6 h; processing moisture ≤0.02 %. Verify the source, grade and conditions.
Equipment setup
Candidate injection-molding recommendations: melt temperature 285 - 310 °C; mold temperature 80 - 110 °C. Verify the source, grade and conditions.
Applications
Review the source and applicable approvals.

Source: the matched material PDF; page numbers refer to the original PDF.

  • Drying temperature:page 2
  • Drying time:page 2
  • Processing moisture:page 2
  • Melt temperature:page 2
  • Mold temperature:page 2