PC-10R-22

Manufacturer:安科聚合物

{'加工': '注塑成型', '认证': '符合RoHS标准'}

Recorded properties

Record date:2026-11-08

PropertyValueUnit
Density1.2g/cm³
Melt flow rate22.0g/10min
Tensile strength60.3MPa
Elongation at break100.0%
Flexural modulus2213.0MPa
Notched impact strength694.0kJ/m²
HDT 1.8MPa137.0°C
Flame rating{'glow_wire_flammability_index_gwfi': '960°C', 'glow_wire_ignition_temperature_gwit': '777°C', 'ul_94_flame_rating': 'V-2'}—

Test standard, specimen condition and source rights are not fully recorded. Values are for preliminary screening only; verify with the manufacturer before design or purchasing decisions.

Grade handling information to verify

The information below was automatically extracted from a material PDF and has not been individually reviewed. It is for preliminary reference only. Verify the exact grade’s manufacturer processing instructions, safety data sheet and equipment procedures before production; do not use candidate values directly as machine settings.

Matched by original PDF filename

Storage
Review the source for packaging, storage and opened-package instructions.
Drying
Candidate injection-molding recommendations: temperature 121 °C; time 3 - 4 h. Verify the source, grade and conditions.
Equipment setup
Candidate injection-molding recommendations: melt temperature 260 - 282 °C; mold temperature 71.1 - 93.3 °C. Verify the source, grade and conditions.
Applications
Candidate application areas in the source: electrical and electronics. Verify the source, exact use and applicable approvals.

Source: the matched material PDF; page numbers refer to the original PDF.

  • Drying temperature:page 1
  • Drying time:page 1
  • Melt temperature:page 1
  • Mold temperature:page 1
  • Application areas:page 2