Polyphenylene ether (PPE) + high impact polystyrene (HIPS)

731S

Manufacturer:NORYL™

良好的表面外观,高延展性,低吸水率,尺寸和水解稳定性

Recorded properties

Record date:2026-11-08

PropertyValueUnit
Density1.08g/cm³
Tensile strength58.0MPa
Elongation at break30.0%
Flexural modulus2420.0MPa
Notched impact strength208.0kJ/m²
HDT 1.8MPa117.0°C

Test standard, specimen condition and source rights are not fully recorded. Values are for preliminary screening only; verify with the manufacturer before design or purchasing decisions.

Grade handling information to verify

The information below was automatically extracted from a material PDF and has not been individually reviewed. It is for preliminary reference only. Verify the exact grade’s manufacturer processing instructions, safety data sheet and equipment procedures before production; do not use candidate values directly as machine settings.

Matched by original PDF filename

Storage
Review the source for packaging, storage and opened-package instructions.
Drying
Candidate injection-molding recommendations: temperature 105 - 110 °C; time 2 - 4 h. Verify the source, grade and conditions.
Equipment setup
Candidate injection-molding recommendations: melt temperature 280 - 310 °C; mold temperature 70 - 95 °C. Verify the source, grade and conditions.
Applications
Review the source and applicable approvals.

Source: the matched material PDF; page numbers refer to the original PDF.

  • Drying temperature:page 1
  • Drying time:page 1
  • Melt temperature:page 1
  • Mold temperature:page 1