Polypropylene

IM 22 63

Manufacturer:TATREN

成核,共聚物,冲击共聚物

Recorded properties

Record date:2026-11-08

PropertyValueUnit
Melt flow rate22.0g/10min
Tensile strength23.0MPa
Tensile modulus1300.0MPa
Elongation at break5.5%
Flexural modulus1250.0MPa
Notched impact strength5.0kJ/m²
HDT 1.8MPa83.0°C

Test standard, specimen condition and source rights are not fully recorded. Values are for preliminary screening only; verify with the manufacturer before design or purchasing decisions.

Grade handling information to verify

The information below was automatically extracted from a material PDF and has not been individually reviewed. It is for preliminary reference only. Verify the exact grade’s manufacturer processing instructions, safety data sheet and equipment procedures before production; do not use candidate values directly as machine settings.

Matched by original PDF filename

Storage
Review the source for packaging, storage and opened-package instructions.
Drying
No drying value was confirmed by extraction; review the source.
Equipment setup
Candidate injection-molding recommendations: melt temperature 190 - 250 °C. Verify the source, grade and conditions.
Applications
Candidate application areas in the source: packaging. Verify the source, exact use and applicable approvals.

Source: the matched material PDF; page numbers refer to the original PDF.

  • Melt temperature:page 1
  • Application areas:page 1