Unspecified
CW50 (CE40)
Manufacturer:Excelloy
Unspecified
Recorded properties
Record date:2026-11-07
| Property | Value | Unit |
|---|---|---|
| Density | 1.15 | g/cm³ |
| Melt flow rate | 30.0 | g/10min |
| Tensile strength | 56.0 | MPa |
| Flexural strength | 83.0 | MPa |
| Flexural modulus | 2100.0 | MPa |
| Flame rating | Unspecified | — |
Test standard, specimen condition and source rights are not fully recorded. Values are for preliminary screening only; verify with the manufacturer before design or purchasing decisions.
Grade handling information to verify
The information below was automatically extracted from a material PDF and has not been individually reviewed. It is for preliminary reference only. Verify the exact grade’s manufacturer processing instructions, safety data sheet and equipment procedures before production; do not use candidate values directly as machine settings.
Matched by original PDF filename
- Storage
- Review the source for packaging, storage and opened-package instructions.
- Drying
- Candidate injection-molding recommendations: temperature 100 - 110 °C; time 2 - 5 h. Verify the source, grade and conditions.
- Equipment setup
- Candidate injection-molding recommendations: mold temperature 50 - 100 °C. Verify the source, grade and conditions.
- Applications
- Review the source and applicable approvals.
Source: the matched material PDF; page numbers refer to the original PDF.
- Drying temperature:page 1
- Drying time:page 1
- Mold temperature:page 1