PA6
SCHULAMID® 6 NV 12 FR
Manufacturer:朗盛工业公司
{'processing': '注塑', 'delivery_form': '颗粒', 'additives': {'release_agent': None, 'special_characteristics': '阻燃'}, 'regional_availability': '北美,欧洲,亚太地区,南美和中美洲,中东/非洲'}
Recorded properties
Record date:2026-11-07
| Property | Value | Unit |
|---|---|---|
| Density | 1.15 | g/cm³ |
| Tensile strength | 70.0 | MPa |
| Tensile modulus | 4200.0 | MPa |
| Elongation at break | 4.0 | % |
| Notched impact strength | 4.0 | kJ/m² |
| HDT 1.8MPa | 90.0 | °C |
| HDT 0.45MPa | 200.0 | °C |
| Vicat softening point | 203.0 | °C |
| Flame rating | V-0 | — |
Test standard, specimen condition and source rights are not fully recorded. Values are for preliminary screening only; verify with the manufacturer before design or purchasing decisions.
Grade handling information to verify
The information below was automatically extracted from a material PDF and has not been individually reviewed. It is for preliminary reference only. Verify the exact grade’s manufacturer processing instructions, safety data sheet and equipment procedures before production; do not use candidate values directly as machine settings.
Matched by original PDF filename
- Storage
- Review the source for packaging, storage and opened-package instructions.
- Drying
- Candidate injection-molding recommendations: temperature 80 °C; time 4 - 6 h. Verify the source, grade and conditions.
- Equipment setup
- Candidate injection-molding recommendations: melt temperature 240 - 260 °C; mold temperature 60 - 90 °C. Verify the source, grade and conditions.
- Applications
- Review the source and applicable approvals.
Source: the matched material PDF; page numbers refer to the original PDF.
- Drying temperature:page 1
- Drying time:page 1
- Melt temperature:page 1
- Mold temperature:page 1