PBT

ELCRIN™ W1000JiQ

Manufacturer:LNP

Recorded properties

Record date:2026-11-07

PropertyValueUnit
Density1.31g/cm³
Melt flow rate23.0g/10min
Tensile strength29.0MPa
Tensile modulus2550.0MPa
Elongation at break140.0%
Flexural modulus2560.0MPa
Notched impact strength4.0kJ/m²
HDT 1.8MPa133.0°C
Vicat softening point168.0°C

Test standard, specimen condition and source rights are not fully recorded. Values are for preliminary screening only; verify with the manufacturer before design or purchasing decisions.

Grade handling information to verify

The information below was automatically extracted from a material PDF and has not been individually reviewed. It is for preliminary reference only. Verify the exact grade’s manufacturer processing instructions, safety data sheet and equipment procedures before production; do not use candidate values directly as machine settings.

Matched by original PDF filename

Storage
Review the source for packaging, storage and opened-package instructions.
Drying
Candidate injection-molding recommendations: temperature 120 °C; time 3 - 4 h; processing moisture ≤0.02 %. Verify the source, grade and conditions.
Equipment setup
Candidate injection-molding recommendations: melt temperature 245 - 260 °C; mold temperature 50 - 75 °C. Verify the source, grade and conditions.
Applications
Review the source and applicable approvals.

Source: the matched material PDF; page numbers refer to the original PDF.

  • Drying temperature:page 1
  • Drying time:page 1
  • Processing moisture:page 1
  • Melt temperature:page 1
  • Mold temperature:page 1