SUS 316L
High ductility and toughness, excellent corrosion resistance.
Key Advantages
- Rigidity
- Corrosion Resistance
Specifications
Lead Time
Standard (2-5 Days)
Thermal Conductivity
16.3 W/m·K
Thermal Expansion
16.0 µm/m·°C
Corrosion Resistance
Excellent
Specific Heat
~500 J/kg·K
Yield Strength
~450 MPa
Tensile Strength
~650 MPa
Density
7.9 g/cm³
Machinability
Good
Application Notes
This material is widely used in high-precision metal 3D printing and CNC machining projects. Its unique combination of properties makes it ideal for complex geometries and functional prototyping.
For specific tolerance requirements or surface finishing options, please refer to our Metal 3D Printing (SLM) Design for Manufacturing (DFM) guide.

Typical Material Application